Discover a professional 3D printing powder supplier
(What is Nickel-Based Superalloy K403)
What is K403 alloy?
Alloy K403 is a cast nickel-based superalloy. The alloy has high high
temperature strength and is widely used for casting guide vanes and working
blades of turbojet, turbopulder, turboshaft and turbofan series engines. The γ'
phase is the main strengthening phase of nickel-based alloys and affects the
high temperature properties of the alloys. The K403 alloy has a higher content
of γ' phase forming elements Al, Ti, etc., so the volume fraction of the γ'
phase in the alloy structure is higher.
Solution treatment of K403 alloy
1. After the alloy undergoes incomplete solution treatment at 1140 and 1180
°C, the microstructure is γ' phase of two sizes; after complete solution
treatment at 1210 °C, air-cooled, 0.2 μm γ' phase is uniformly precipitated.
With the increase of the solution temperature, the primary γ' phase gradually
decreases, and the dendrite structure becomes inconspicuous.
2. For the alloy after solution treatment at 1190 ℃ for 4h, the size of γ'
phase particles changes little after aging at 900, 940 ℃ for 16h, but the
distribution is more uniform; after aging at 980 ℃ for 16h, the particle size of
γ' phase decreases It became larger to 0.3-0.6 μm, and the shape changed from
square to irregular, nearly circular. After aging, the tensile properties and
hardness of the alloy are improved.
3. The alloy obtained the relative maximum tensile strength and room
temperature hardness after aging at 940℃. The recommended heat treatment process
for K403 alloy is 1190 ℃, 4h, AC+ 940 ℃, 16h, AC.
About 3dprintingpassion
3dprintingpassion is a trusted global chemical material supplier & manufacturer with
over 12 years experience in providing super high-quality chemicals and
Nanomaterials. The company export to many countries, such as USA, Canada,
Europe, UAE, South Africa, Tanzania,
Kenya,Egypt,Nigeria,Cameroon,Uganda,Turkey,Mexico,Azerbaijan,Belgium,Cyprus,Czech
Republic,Brazil, Chile, Argentina, Dubai, Japan, Korea, Vietnam, Thailand,
Malaysia, Indonesia, Australia,Germany, France, Italy, Portugal etc. As a
leading nanotechnology development manufacturer, 3dprintingpassion dominates the market.
Our professional work team provides perfect solutions to help improve the
efficiency of various industries, create value, and easily cope with various
challenges. If you are looking for K403 powder, please send an email to:
sales2@nanotrun.com
(What is Nickel-Based Superalloy K403)